US$ 19.99
(Flux-Cored) Welding Processes MIG (GMAW)
enhances operational efficiency
consider the 0
Lincoln OEM HOSE
5 low-alloy low-hydrogen SMAW electrode with 90 ksi minimum tensile and military-spec (MIL) chemistry tightly controlled for low temperature impact toughness on HY-80 / HY-100 high-strength steels in shipbuilding
Lincoln ED030975 Outershield 91K2-H Flux-Cored (FCAW-G) Welding Wire, 0.045 in, 25 lb Spool Package Size:0.052 in · 25 lb Spool (Flux-Cored) Welding Processes MIG (GMAW)Offers superior puddle control in all positions, virtually effortless slag removal, and excellent bead wetting. It can potentially reduce the level of preheat normally used on crack sensitive steels. Features Designed for welding with 75 95% Argon Balance CO2 shielding gas Capable of producing weld deposits with tensile strength exceeding 620 MPa (90 ksi) Use on high strength, low alloy steel applications H8 diffusible hydrogen levels
US$ 19.99
US$ 20.99
US$ 18.99
US$ 47.99
US$ 333.50
US$ 382.33
US$ 300.10
US$ 194.00